Journal · Process
An hour per inch
The rule I was taught is an hour in the steam box for every inch of thickness. It is a good rule. It is also a starting point, which is something the person who taught it to me said only once, quietly, after I’d cracked my third arm bow.
Timber that has been drying for too long resists. Timber with a run-out in the grain will tell you about it halfway round the former. Most of what I know about bending I learned by listening for the small sound wood makes just before it fails.
This journal is partly for you, so you can see how a chair gets made. It is also for me, so that the things my hands have learned get written down somewhere.